| Anti-glare and hard coating are applied on the surface of polarizer to control the reflection of fluorescent light and the sunny light and to prevent scratch in the process or treatment. |






|
W/O Treatment
|
Hard Coat
|
Conventional Type
|
Highly Minute Type
|
AGA1
|
AGA2
|
Haze
|
-
|
-
|
26
|
13
|
40
|
60Glossiness
|
95
|
88
|
24
|
35
|
50
|
Glare
|
-
|
-
|
Δ
|
Δ
|

|
Resistance to Scratch
|
×
|

|

|

|

|
Surface Hardness
|
-
|
3H
|
3H
|
3H
|
3H
|
|
: Most Excellent Ο : Excellent Δ : Normal × : Inferior
|

Haze:Measuring method of Haze is according to JIS K6714
60 degree Glossiness:Measuring method of 60 degree glossiness is according to JIS Z8741
Glare:Measuring method of glare is according to cell at 200ppi
Resistance to Scratch:For the test of resistrance to scratch, steel wool (#0000) is used
Surface Hardness:Measuring method of surface hardness is according to JIS K5400. Pressure should be 500g.
|
|
 |
|
 |