Anti-reflection treatment shall be applied on the surface of polarizer, to improve the optical performance and visible performance of display. Furthermore, dirt-preventing layer is applied on the top of anti-reflection surface so as to make wipe out easily oily dirtiness such as fingerprints.
There are two choice of this type. The one is the type of performance priority (spattering), and the other is cost priority (coating). |






|
Haze
|
5degree Reflective Charactertic Data
|
Transmittance
|
P.E.
|
Y
|
x
|
y
|
Single
|
Parallel
|
Crossed
|
Plain
|
-
|
4.5
|
0.31
|
0.31
|
43.0
|
37.0
|
0.003
|
99.99
|
ARP
|
-
|
0.4
|
0.22
|
0.11
|
44.2
|
39.0
|
0.008
|
99.98
|
LRP
|
-
|
1.26
|
0.33
|
0.30
|
43.9
|
38.4
|
0.010
|
99.97
|
AGLRP1
|
9
|
0.82
|
0.30
|
0.30
|
43.4
|
37.8
|
0.009
|
99.98
|
|


|
 |
|
 |